Cmyk White PE PP BOPP Film Printing UV LED Curing UV Ink
HomeHome > Products > UV INK > Cmyk White PE PP BOPP Film Printing UV LED Curing UV Ink
Cmyk White PE PP BOPP Film Printing UV LED Curing UV Ink

Cmyk White PE PP BOPP Film Printing UV LED Curing UV Ink

CMYK White PE PP BOPP Film Printing UV Led Curing UV Ink Product DescriptionWSL series is a Led offset printing Ink. It
Basic Info.
Model NO. WSL-5000
Custom Sample Available
Application Paper Bag
Shelf Life 2 Years
Density High Color Density
Certificates FDA, RoHS
Fluidity Good Fluidity
Stock Available
Deliver Time Within One Week
Odor 0 Grade
Features Bright Color
Viscosity 22-28 Seconds with 3# Zahn Cup
Waterproof 0 Grade
Wear Risistance 0 Grade
pH Value 8.2-9.0
Transport Package Barrel, Pallet
Specification 1kg/tin
Trademark Oriental Colors
Origin China
HS Code 32159090
Production Capacity 700000 Kg/Month
Product Description
CMYK White PE PP BOPP Film Printing UV Led Curing UV Ink
Product DescriptionWSL series is a Led offset printing Ink. It is most used in paper printing. It has big water supplying tolerance and machine safety.After printing It can be proceeded the next step instant after drying by Led. No back printing or paste. Good Adhension, bright color, full printing, good transfering, with high network clerity. VOCs is food grade, and can be used in food and wine packaging directly. It offers good flexibility for the printing machine. High transparency.
Color Ink

Cmyk White PE PP BOPP Film Printing UV LED Curing UV Ink

ItemParameterItemParameter
Appearance(Visible)Four color and various spot color in paste conditionsolid content (weightlessness)99.8%
Viscosity(CPS/25 ºC)90 000 to 150000Adhesion100/100
Anti flying inkexcellentfineness≤5
VOCs≤0.003 mmflexibilityfold without burst
Fluidity30-32 mmviscosity10
Emulsification value30tinting strength100/100
Transparencyexcellencyyellowing grade(UV)≥4.5
Shelf life(25 ºC)One yearcuring MethodLED

Cmyk White PE PP BOPP Film Printing UV LED Curing UV Ink


Cmyk White PE PP BOPP Film Printing UV LED Curing UV Ink


Cmyk White PE PP BOPP Film Printing UV LED Curing UV Ink


Q1:How to avoid color difference?
A: Use new ink each time. Avoiding water adding, if it is needful, try to add little each time and mix evenly. Use the same substrate each time(the base color of the substrate will cause color difference. Maintain the printing press, anilox roller, andscraper in time; clean the ink box in time.Q2: Why there is odor from the ink?
A: Tap water will shorten the ink shelf time. It will deteriorate easier if too much tap water added. Stock the ink in sealed condition and in ventilated place.Q3: How to solve the edge fluffing problem?
A: In low printing speed, restart the press or tune the press until the scraping plate appears. In normal high speed printing, add slowing dry agent or stabilizer to solve the fluffing problem.Q4: What are the reasons for the printed words are too slim and not clear?
A: The printing is too slow but drying is fast, poor converting. Printing pressure is too big and the ink loading is too much.Q5: The printing drying condition is not good, what are the reasons?
A: The ambient temperature is too low; the humidity is too high;the power of the drying tunnel or infrared lamp is low. Substrate surface is too smooth, and the ink absorption deviate.Q6: The ink become thick after long storage, how can I reuse it?
A: Generally speaking, if stored in our suggested way, the ink will keep in good condition. It become thick because it is stored unsealed and the water volatilized. you can add some stabilizer and water, stir evenly and filter. Then you can use again.